I watched a 3D printing youtuber say that Adam Savage said 20% but 10% is what he uses.

I have never seen my sunlu dryer show anything bellow 23% even after days of use and I have no idea how to achieve 10 without cooking the filament.

  • ShadowRam@fedia.io
    link
    fedilink
    arrow-up
    2
    ·
    10 months ago

    You solved that via annealing and releasing the stress in the PLA, not by drying it.